Química Nova (Jun 2000)

Extração de ferro de esmectita brasileira com emprego do método ditionito-citrato-bicarbonato Iron extraction from Brazilian smectite by dithionite-citrate-bicarbonate method

  • Sidnei Quezada M. Leite,
  • Carlos Henrique A. Colodete,
  • Lídia Chaloub Dieguez,
  • Rosane A. S. San Gil

DOI
https://doi.org/10.1590/S0100-40422000000300002
Journal volume & issue
Vol. 23, no. 3
pp. 297 – 302

Abstract

Read online

A natural clay from Campina Grande region (Paraíba, Brazil), with 8.57% of Fe2O3, was used to study the most appropriate condition to carry out the iron extraction, without altering the clay structure in a significant way. Samples were treated with the Dithionite-Citrate-Bicarbonate method (DCB) for 30 and 120 minutes (pH=9.1), and also with citric acid (pH=1.8; time=15min), at 75°C. Conductivity measurements, X-ray fluorescence, X-ray diffraction, energy-dispersive spectrometry, electron-diffraction with transmission electron microscopy and textural evaluation by nitrogen adsorption were done. The treatment in a basic medium was more selective for iron removal than in acid condition. The time of 30 minutes, with 1.6 g Na2S2O4/10 g clay, was the best condition for the iron extraction.

Keywords