This article deals with the development of a new composition of a polymer composition for dressing cotton yarn. The optimal concentration of the dressing polymer composition, which is 50 g/kg, against the starch-based dressing is 70 g/kg, i.e., the consumption of starch is reduced by 25-30%. It is experimentally established that the concentration of the dressing, which has a significant impact on the cost of the dressing, varies within 45-50 g/kg of the composition, while the true glue remained at the same level.