Eurasian Journal of Physics and Functional Materials (Jun 2021)
The nature of intrinsic recombination emission in SrSO4 irradiated with ultraviolet photons
Abstract
The synthesized SrSO4 crystalline powders were irradiated at photon energies from 6 ÷ 12 eV, in the temperature range from 15 ÷ 300 K. The investigation was carried out by the methods of atomic absorption, luminescence and vacuum ultraviolet spectroscopy. Intrinsic emissions were found at 3.7-3.8 eV, 4.2-4.6 eV and 4.9-5 eV, and long-wavelength recombination emissions at 2.6-2.7 eV and 2.9-3.0 eV. The synthesized SrSO4 crystalline powders were irradiated at photon energies from 6 ÷ 12 eV, in the temperature range from 15 ÷ 300 K. The investigation was carried out by the methods of atomic absorption, luminescence and vacuum ultraviolet spectroscopy. Intrinsic emissions were found at 3.7-3.8 eV, 4.2-4.6 eV and 4.9-5 eV, and long-wavelength recombination emissions at 2.6-2.7 eV and 2.9-3.0 eV.
Keywords