Abstract

Read online

Electron backscatter diffraction, five parameter analysis, overlap-pole-figure analysis and near coincident site analysis were used to investigate the interface character distributions of WC/WC grain boundaries and WC/Co phase boundaries in WC/Co cemented carbides under different heat treatment states. The results show that the WC/WC Σ2 grain boundaries with a fraction of 4.5% are generated in the oil-quenched sample after high temperature sintering. The fraction of Σ2 boundaries with interface matching features of {101¯0}/{101¯0} is 2.6%.The cobalt in this sample is basically face-centered-cubic structure, and the interface with the interface inter-connection features of {101¯0}WC/{001}Co,{101¯0}WC/{110}Co and {112¯0}WC/{110}Co is the main part of the WC/Co phase boundary. After tempering at 800 ℃, the samples with atmosphere protection and slow cooling in the furnace have the proportion and characteristics of WC/WC Σ2 grain boundaries, which are very close to those of oil-quenched samples.The cobalt in this sample is primarily hexagonal structure, and the interface with the interface inter-connection features of {101¯0}WC/{101¯0}Co and {112¯0}WC/{112¯0}Co is the main part of the WC/Co phase boundary.

Keywords