Abstract It is of interest to develop wide-temperature domain damped hydrophobic materials. In this paper, we designed incorporating bio-based phenolic resin into the IIR matrix and introducing dibenzyl fork acetone (DBA) into the main chain structure with sodium hydroxide activation to construct three-dimensional network. In this paper, we designed incorporating bio-based phenolic resin into the IIR matrix and introducing dibenzyl fork acetone (DBA) into the main chain structure with sodium hydroxide activation to construct three-dimensional network. The added bio-based phenolic resin has reticulated structure blended with butyl rubber, combined with sodium hydride activation-modified IIR. The results show that sodium hydride activated modification of DBA is introduced into the main chain structure of IIR by infrared and 1H NMR analysis. The material hydrophobic is realized by the introduction of DBA with static water contact angle of 103.5°. The addition of 10phr lignin-based phenolic resin (LPF) is compatible with IIR, and the torque can reach 7.0 N-m. The tensile elongation of the modified butyl rubber composite can reach 2400% with tensile strength up to 11.43 MPa, while the damping factor can reach 0.37 even at 70 °C. The thermal stability of the composites is enhanced with mass retention rate of 28%. The bio-based PF/NaH activation-modified butyl rubber damping material has potential applications in damping hydrophobicity with wide temperature range.

Keywords