Archives of Metallurgy and Materials (Sep 2015)

Influence Of Temperature On The Rate Of Copper Recovery From The Slag Of The Flash Direct-To-Blister Process By A Solid Carbon Reducer

  • Madej P.,
  • Kucharski M.

DOI
https://doi.org/10.1515/amm-2015-0289
Journal volume & issue
Vol. 60, no. 3
pp. 1663 – 1672

Abstract

Read online

The aim of the work was to investigate the influence of temperature on the rate of copper removal from the obtained slag from the flash direct-to-blister process by means of a carbon reducer. The slag used in this work was taken from the direct-to-blister Outokumpu flash furnace at the smelter in Głogów, and graphite penetrators were used as the slag reducers. The experiment was carried out at 1573 K, 1623 K and 1673 K. It was found that the rate of the de-coppering process of the “Głogów” slag increased with the increase of temperature.