Abstract

Read online

This work presents the results of the homogenization of the color of sapwood and false heartwood Fagus sylvatica L. into a uniform color shade due to the influence of the temperature of saturated moist air and saturated water steam in individual steaming modes. The results of analyses of the influence of temperature within 24 h point out the different changes in the color of the sapwood and the wood of the false heartwood when the uniform color of the beech wood is achieved by the steaming process. By steaming beech wood with a false heartwood saturated with moist air at a temperature of tI = 95 °C during τ = 24 h, the color of the sapwood does not merge with the color of the wood of the false heartwood. The sapwood darkens and, on the other hand, the wood of the false heartwood slightly lightens, while the significant color contrast is removed, but the color homogenization in the individual zones does not occur. The unification of the colors in individual zones occurs during the steaming process at a temperature of saturated water steam tII ≈ 105 °C in 18 h, where the resulting brown color is identified in the color space CIE L*a*b* by the values of the lightness L* = 61.3 ± 2.2 and of the red color a* = 12.4 ± 1.3 and yellow color b* = 19.5 ± 1.4. The most pronounced homogenization of the color occurs through the steaming process at a temperature of saturated water steam tIII ≈ 120 °C, where the wood acquires a uniform dark brown–gray color in a time of τ ≈ 9 h steaming. The coordinates of the color-homogenized steamed beech wood are L* = 55.9 ± 1.9, a* = 12.3 ± 1.2, and b* = 19.6 ± 1.3. The unification of the colors by the steaming process is achieved by darkening both the sapwood and the wood of the false heartwood. In the overall color homogenization, the sapwood and the wood of the false heartwood do not participate equally in the steaming process. While the total color difference between the sapwood and a color homogenized state is quantified by the value ∆EtI* = 8, ∆EtIII* = 22.7, the total color difference in the wood with a false heartwood is only ∆EtI* = 1.9, ∆EtIII* = 11.8.

Keywords