Polímeros (Sep 2017)

Evaluation of degree of conversion, microtensile bond strength and mechanical properties of three etch-and-rinse dental adhesives

  • Samantha Ariadne Alves de Freitas,
  • Marco Daniel Septimo Lanza,
  • Karina Kato Carneiro,
  • Alessandro Dourado Loguercio,
  • José Bauer

DOI
https://doi.org/10.1590/0104-1428.02316
Journal volume & issue
Vol. 27, no. 3
pp. 230 – 236

Abstract

Read online

Abstract This study evaluated microtensile bond strength (µTBS), degree of conversion, modulus of elasticity and ultramicrohardness of three etch-and-rinse adhesives systems. The materials evaluated were: Ambar (FGM), Optibond (Kerr) and Magic Bond (Vigodent). The degree of conversion was analyzed by FTIR/ATR. To evaluate bond strength (μTBS) in dentin, 15 teeth (n = 5) were restored and sliced to obtain the specimens (0.8mm2). The dynamic ultra microhardness tester was used to evaluate the hardness and modulus of elasticity. The Magic Bond adhesive system showed lower µTBS than Ambar and Optibond (p <0.001). For degree of conversion, comparisons between groups of adhesive systems evaluated showed statistically significant difference (p<0.001), with higher values for Ambar and Optibond when compared a Magic Bond. For modulus of elasticity and ultramicrohardness, Ambar and Magic Bond showed lower values than Optibond. The best results in all properties evaluated were obtained by the Optibond adhesive system.

Keywords