Damage and failure analysis of composite stiffened panels under low-velocity impact and compression after impact with damp-heat aging

  • Du Changmei,
  • Li Hanhua,
  • Yan Shi,
  • Zhang Qiuhua,
  • Jia Jiale,
  • Chen Xixi

DOI
https://doi.org/10.1515/secm-2022-0159
Journal volume & issue
Vol. 29, no. 1
pp. 378 – 393

Abstract

Read online

The low-velocity impact and compression after the impact of the composite stiffened panels were carried out after damp-heat aging. The experimental results show that reinforcing the ribs can enhance the impact resistance of test pieces after damp-heat aging. After impacting, the specimens were tested in an axial compression. The results show that the ultimate bearing capacity of the specimen is also affected by different located positions of the impact and different aging times. Compared with the intact specimen, the ultimate load-bearing capacity was reduced to 16.83, 12.10, and 17.10% with the specimen aging for 0, 45, and 90 days, respectively, while the impact position located at the intersection of longitudinal and transverse bars has the greatest influence on the damp-heat aging of specimens.

Keywords