Metalurgija (Jan 2007)
The Balance of Titanium and Vanadium in the Blast Furnace with the Use of Sinter Containing a Titanium-Vanadium-Magnetite Concentrate
Abstract
The investigation concerned the use of sinter containing a titanium-vanadium-magnetite concentrate for the production of pig iron. Sinter containing 0,46 to 0,51 % TiO2 and 0,056 to 0,060 % vanadium was used for pig iron production in the blast furnace. Introducing 200 kg of this concentrate to the1 Mg sinter mix did not cause any deterioration of sinter quality.