Ecotoxicology and Environmental Safety (Nov 2022)

Effect of polar/non-polar facets on the transformation of nanoscale ZnO in simulated sweat and potential impacts on the antibacterial activity

  • Xiang Zhang,
  • Xiaoting Qian,
  • Jie Tang,
  • Nali Zhu,
  • Zhigang Li,
  • Jianjie Fu,
  • Lingxiangyu Li,
  • Yawei Wang

Journal volume & issue
Vol. 246
p. 114187

Abstract

Read online

The use of nanoscale zinc oxide (n-ZnO) in the personal care products would cause interactions between n-ZnO and human sweat. Facet engineering has been applied to n-ZnO to improve its activity. Nevertheless, it is not clear whether the exposed facet would affect transformation of n-ZnO in sweat. Herein, we prepared ZnO nanoneedles with the dominant (1010) non-polar facet (i.e., ZnO-1010) and ZnO nanoflakes with the dominant (0001) polar facet (i.e., ZnO-0001), respectively. We found that n-ZnO can undergo chemical transformation in the simulated sweat within 168 h or 24 h, transforming into amorphous materials and Zn3(PO4)20.4 H2O and/or Na(ZnPO4)·H2O. Given the rate constant (e.g., 0.093 h−1 for ZnO-0001 vs. 0.033 h−1 for ZnO-1010) of ZnO depletion and components of the precipitate from the simulated sweat, nevertheless, the transformation is highly dependent on the dominant exposed facet of n-ZnO. The ZnO-0001 relative to ZnO-1010 would likely undergo chemical transformation, demonstrating that the (0001) polar facet compared to (1010) non-polar facet had a superior activity to the dihydrogen phosphate anions in the simulated sweat, which is supported by density functional theory calculations. The chemical transformation can affect the antibacterial activity of n-ZnO to E. coli, moderating the toxicity due to a great decrease in the concentration of the dissolved zinc. In total, our findings provided insights into the facet-dependent transformation for n-ZnO in the simulated sweat, improving our understanding of potential risk of n-ZnO.

Keywords