Archives of Metallurgy and Materials (Jun 2016)

Reduction of Industrial Nickel Oxides with a Hydrogen Bearing Gas Between 523 and 673 K

  • G. Plascencia

DOI
https://doi.org/10.24425/122404
Journal volume & issue
Vol. vol. 63, no. No 2

Abstract

Read online

Reduction of three industrial nickel oxides (Goro, Tokyo and Sinter 75) with a hydrogen bearing gas was revisited in the temperature interval from 523 to 673 K (250 to 400°C). A pronounced incubation period is observed in the temperature interval tested. This period decreases as the reduction temperature increases. Thermogravimetric data of these oxides were fitted using the Avrami-Erofeyev kinetic model. The reduction of these oxides is controlled by a nucleation and growth mechanism of metallic nickel over the oxides structure. Rate kinetic constants were re-evaluated and the activation energy for the reduction of these oxides was re-calculated.

Keywords