Abstract
Bismuth (III) oxide was obtained by electrodeposition, followed by thermal treatment in air environment. The applied electrodeposition current density and electrode potential affect the surface morphology and chemical composition of the obtained deposit before and after the thermal treatment at 350°C, as well as its crystal structure after the thermal treatment at 350°C. The listed parameters affect the deposit’s morphology after the thermal treatment at 600°C, but do not affect its chemical composition and crystal structure. The conclusion is that investigated working electrode material does not affect the characteristics of synthesized material. [Project of the Serbian Ministry of Education, Science and Technological Development, Grant no. 34008]