Journal of Thermal Science and Technology (Jul 2012)

Quantification of the Existence Ratio of Non-Adhesion Grain Boundaries and Factors Governing the Strength of Coke Containing Low-Quality Coal

  • Tetsuya KANAI,
  • Yoshiaki YAMAZAKI,
  • Xiaoqing ZHANG,
  • Ataru UCHIDA,
  • Yasuhiro SAITO,
  • Masakazu SHOJI,
  • Hideyuki AOKI,
  • Seiji NOMURA,
  • Yukihiro KUBOTA,
  • Hideyuki HAYASHIZAKI,
  • Shigeto MIYASHITA

DOI
https://doi.org/10.1299/jtst.7.351
Journal volume & issue
Vol. 7, no. 2
pp. 351 – 363

Abstract

Read online

“Non-adhesion grain boundaries” are formed when low-quality coal grains do not adhere to other grains in the carbonization process because of the low dilation of coke. To better understand the effects of non-adhesion grain boundaries on coke strength, the relationship between the existence ratio of non-adhesion grain boundaries and coke strength was investigated quantitatively. The existence ratio of non-adhesion grain boundaries were measured quantitatively by observing the fracture cross-section of coke using scanning electron microscopy (SEM). Coke strength was measured with a diametral-compression test and an I-shape drum index test. As a result, non-adhesion grain boundaries increased with an increase in the blending ratio of low-quality coal. In particular, non-adhesion grain boundaries increased rapidly when the blending ratio of low-quality coal was over 50%. When the ratio was less than 50%, low-quality coals adhered to other caking coal. However, not many low-quality coals adhered to other caking coals when the ratio was over 50%. The tensile strength of coke was not affected by the porosity of coke. However, the tensile strength and the drum index were affected by the existence ratio of non-adhesion grain boundaries. Tensile strength decreased rapidly even for a few non-adhesion grain boundaries because significant defects caused a fracture in the diametral-compression test. However, the I-shape drum index decreased linearly with the existence ratio of the non-adhesion grain boundaries because many fractures occurred during 600 rotations in the drum. The strength of coke containing low-quality coal is governed by the existence ratio of non-adhesion grain boundaries rather than mean values such as the porosity of coke.

Keywords