Archives of Foundry Engineering (Jun 2016)

Micro-jet Cooling by Compressed Air after MAG Welding

  • Węgrzyn T.,
  • Piwnik J.,
  • Tarasiuk W.,
  • Stanik Z.,
  • Gabrylewski M.

DOI
https://doi.org/10.1515/afe-2016-0036
Journal volume & issue
Vol. 16, no. 2
pp. 111 – 114

Abstract

Read online

The material selected for this investigation was low alloy steel weld metal deposit (WMD) after MAG welding with micro-jet cooling. The present investigation was aimed as the following tasks: analyze impact toughness of WMD in terms of micro-jet cooling parameters. Weld metal deposit (WMD) was first time carried out for MAG welding with micro-jet cooling of compressed air and gas mixture of argon and air. Until that moment only argon, helium and nitrogen and its gas mixture were tested for micro-jet cooling.

Keywords