AIP Advances (Nov 2015)

Improved room-temperature-selectivity between Nd and Fe in Nd recovery from Nd-Fe-B magnet

  • Y. Kataoka,
  • T. Ono,
  • M. Tsubota,
  • J. Kitagawa

DOI
https://doi.org/10.1063/1.4935570
Journal volume & issue
Vol. 5, no. 11
pp. 117212 – 117212-7

Abstract

Read online

The sustainable society requires the recycling of rare metals. Rare earth Nd is one of rare metals, accompanying huge consumption especially in Nd-Fe-B magnets. Although the wet process using acid is in practical use in the in-plant recycle of sludge, higher selectivity between Nd and Fe at room temperature is desired. We have proposed a pretreatment of corrosion before the dissolution into HCl and the oxalic acid precipitation. The corrosion produces γ-FeOOH and a Nd hydroxide, which have high selectivity for HCl solution at room temperature. Nd can be recovered as Mn2O3-type Nd2O3. The estimated recovery-ratio of Nd reaches to 97%.