Teshugang (Mar 2024)

Effect of S on Solidification Behavior of Cast Superalloy K417G

  • Yang Yaqian , Xing Weiwei , Ding Leilei , Ma Yingche

DOI
https://doi.org/10.20057/j.1003-8620.2023-00217
Journal volume & issue
Vol. 45, no. 2
pp. 30 – 38

Abstract

Read online

The effects of 0.0001%,0.0018% and 0.0037% S content on the solidification characteristics of K417G alloy were studied by isothermal solidification experiment in the temperature range of 1340-1230 ℃. The results show that S can reduce the solidus temperature of the alloy and enlarge the solid-liquid two phase region. When the S content increases from 0.0001% to 0.0037%, the solidus temperature of the alloy decreases from 1255 ℃ to 1245 ℃. During the solidification process, the S element segregates in the liquid phase and precipitates out as the Y phase in the final solidification zone. And S promotes the enrichment of Al and Cr elements at the solid-liquid interface. At the same isothermal temperature, the increase of S content promotes the increase of the volume fraction of MC carbide,γ+γ΄ eutectic and Y phase, and has little effect on the morphology and precipitation temperature of MC carbide and γ+γ΄ eutectic, but the precipitation temperature of the Y phase is increased from 1230 ℃ to 1240 ℃.

Keywords