Polish Journal of Chemical Technology (Dec 2019)

Application of Taguchi method in the optimization of synthesis of cellulose-MgO bionanocomposite as antibacterial agent

  • Safaei Mohsen,
  • Taran Mojtaba,
  • Imani Mohammad Moslem,
  • Moradpoor Hedaiat,
  • Rezaei Farzad,
  • Jamshidy Ladan,
  • Rezaei Razieh

DOI
https://doi.org/10.2478/pjct-2019-0047
Journal volume & issue
Vol. 21, no. 4
pp. 116 – 122

Abstract

Read online

In this study, optimal conditions to form cellulose-MgO nanocomposite with antibacterial properties were evaluated. Applying the Taguchi method, 9 experiments were designed and the effects of different concentrations of biopolymers cellulose (0.5, 1 and 2 mg/ml), MgO nanoparticles (2, 4 and 8 mg/ml) and stirring times (30, 60 and 90 min) on antibacterial activity of synthesized nanocomposites were assessed. The characterizations of products were investigated by dynamic light scattering (DLS), raman spectroscopy, scanning electron microscope (SEM), thermogravimetric analysis (TGA) and differential thermal analysis (DTA). The results showed that the nano-composite produced in the conditions of experiment 9 (MgO 8 mg/ml, cellulose 2 mg/ml and stirring time of 60 min) has the strongest antibacterial activity. The outcomes of both methods of colony forming units (CFU) and disc diffusion indicated that the antibacterial activity of cellulose-MgO nanocomposite was significantly higher than its components (P <0.05). Thermal analysis indicated improvement in the thermal stability of the cellulose biopolymer after the formation of the nanocomposite. Due to the improvement of the antibacterial properties of cellulose-MgO nanocomposite compared to its components, we can use it as a new antibacterial agent in the fields of pharmaceutical, medicine and dentistry.

Keywords