Effects of heat treatment on properties of multi-element low alloy wear-resistant steel
Abstract
The paper has studied the mechanical properties and heat treatment effects on multi-element low alloy wear-resistant steel (MLAWS) used as a material for the liner of rolling mill torii. The results show that when quenched at 900-920℃ and tempered at 350-370℃, the MLAWS has achieved hardness above 60 HRC, tensile strength greater than 1 600 MPa, impact toughness higher than 18J/cm2 and fracture toughness greater than 37 MPa