Thresholds of explosive degradation of PETN with different additives in the laser exposure were measured, with the additives being Al, Al-C, Ni, Co, «Kemerit ®», nanoparticles with different content Al/Al2O3. The expansion ve- locity of the explosion products of certain materials was measured. Thresholds of explosive decomposition were meas- ured with regard of the initial temperature and the melted extruded samples of Ni-C and Al. In prersence of 0.1 % Al as additive, the sensitivity is shown to decrease, as compared to samples containing no additives. This allows us to consid- er this part of mixtures a promising material for light detonators.