Science and Engineering of Composite Materials (Jan 2019)
Negative effect of clay fillers on the polyvinyl alcohol biodegradation: technical note
Abstract
This work focuses on polyvinyl alcohol (PVA) biodegradation in the presence of mineral clays in an aqueous aerobic environment. PVA with a degree of hydrolysis of 88% and 72% was used for the experiments. The selected group of mineral clays (nanofillers for polymers) of montmorillonite (MMT) Cloisite® Na+; organo-modified montmorillonite (OMMT) Cloisite® 20A, Cloisite® 30B; waste kaolin; kaolin; and zeolites were prepared by synthesis of the aforementioned kaolins. The level of biodegradation was measured using a respirometer, Micro-Oxymax, and evaluated according to CO2 production. Results of this test indicate a negative effect on PVA biodegradability in the presence of MMT Cloisite® Na+ and Cloisite® 30B. It has been found that PVA biodegradability in the presence of no adapted inoculum was adversely affected by the biocidal effects of the organic modifier of Cloisite® 30B. In this case, PVA 88-8 biodegradation decreased by 71% and PVA 72-10 biodegradation dropped by 58%. Furthermore, the sorption of PVA on the Cloisite® Na+ in the range of 40%–45% was demonstrated in the following research.
Keywords