High Temperature Materials and Processes (Nov 2016)

Reduction Smelting Low Ferronickel from Pre-concentrated Nickel-Iron Ore of Nickel Laterite

  • Zhu Deqing,
  • Zhou Xianlin,
  • Luo Yanhong,
  • Pan Jian,
  • Bai Bing

DOI
https://doi.org/10.1515/htmp-2015-0025
Journal volume & issue
Vol. 35, no. 10
pp. 1031 – 1036

Abstract

Read online

The research of smelting low ferronickel from pre-concentrate nickel-iron ore with 2.76 % Ni and 38.00 % Fetotal was carried out to find an effective way for stainless steel enterprises to use the low-nickel laterite reasonable. The results show that Ni and Fe both have a certain degree of enrichment, and impurities and harm elements have different degrees of reduction after pre-concentration of nickel-iron ore. Most valuable metal did not compound with impurities which greatly accelerated the speed and extent of melt separation reduction. Good alloy of 6.58 % Ni with the overall recoveries of 93.38 % and 89.95 % Fetotal with the overall recoveries of 89.57 % was manufactured under the following conditions: 10 % coke, 1.0 binary basicity, 18 % MgO and 3 % Al2O3 in slag, melting at 1,550 °C for 10 min. The product can be used for the feed of producing stainless steel.

Keywords